1
| QUIKLIME - | HYDRATEDLIME HAVINING ACTIVE CAO CONTENT MINIMMUM 85% Specification : Avilable CaO + 85%, Magnesium as MgO should be less than 0.5%, silica as SiO2 should be less than 0.5%, Iron as Fe203 should be less than 0.5%, Aluminina as AI203 should be less than 0.5%, Unburnt/dead burnt lime should be less than 0.5%, Manganese as Mn203 should be less than 0.03%, Lime should be highly porous, light in weight and slakes quickly to form calcium hydroxide, Lime should immediately swells up and breaks if water is poured over a lump | MTS | 1600 |